Home
>
Material
EN 10083-2-2006
Steels for quenching and tempering. Part 2:Technical delivery conditions for non alloy steels
Material Designation
Chemical Composition (%)
C45E
(
1.1191
)
Min
Max
C35E
(
1.1181
)
Min
Max
C60E
(
1.1221
)
Min
Max
C55E
(
1.1203
)
Min
Max
C50E
(
1.1206
)
Min
Max
C35
(
1.0501
)
Min
Max
C40
(
1.0511
)
Min
Max
C45
(
1.0503
)
Min
Max
C55
(
1.0535
)
Min
Max
C60
(
1.0601
)
Min
Max
C22E
(
1.1151
)
Min
Max
C22R
(
1.1149
)
Min
Max
C35R
(
1.1180
)
Min
Max
C40E
(
1.1186
)
Min
Max
C40R
(
1.1189
)
Min
Max
C45R
(
1.1201
)
Min
Max
C55R
(
1.1209
)
Min
Max
C60R
(
1.1223
)
Min
Max
28Mn6
(
1.1170
)
Min
Max
C50R
(
1.1241
)
Min
Max
For Reference Only