Home > Material
1.1223
Standard DIN 17200-1987
Standard EN 10083-2-2006 Steels for quenching and tempering. Part 2:Technical delivery conditions for non alloy steels
Standard DIN 17204-1990
Standard NF EN 10083-2-2006 Tempered non-alloy structural steel


Chemical Composition(%)


Standard Material Designation Chemical Composition (%)
EN 10083-2-2006
Steels for quenching and tempering. Part 2:Technical delivery conditions for non alloy steels
C60R
(1.1223)
 
Min
Max
DIN 17200-1987 Cm60
(1.1223)
 
Min
Max
NF EN 10083-2-2006
Tempered non-alloy structural steel
C60R
(1.1223)
 
Min
Max
DIN 17204-1990 Cm60
(1.1223)
 
Min
Max
For Reference Only