Home
>
Material
1.1206
Standard
DIN 17200-1987
Standard
EN 10083-2-2006
Steels for quenching and tempering. Part 2:Technical delivery conditions for non alloy steels
Standard
EN 10132-2021
Cold rolled narrow steel strip for heat treatment - Technical delivery conditions
Standard
NF EN 10083-2-2006
Tempered non-alloy structural steel
Chemical Composition
(%)
Standard
Material Designation
Chemical Composition (%)
EN 10083-2-2006
Steels for quenching and tempering. Part 2:Technical delivery conditions for non alloy steels
C50E
(
1.1206
)
Min
Max
DIN 17200-1987
Ck50
(
1.1206
)
Min
Max
NF EN 10083-2-2006
Tempered non-alloy structural steel
C50E
(
1.1206
)
Min
Max
EN 10132-2021
Cold rolled narrow steel strip for heat treatment - Technical delivery conditions
C50E
(
1.1206
)
Min
Max
For Reference Only