Standard EN 10084-1998 Case hardening steels. Technical delivery conditions
Standard DIN EN ISO 683-3-2019 Heat-treatable steels,alloy steels and free-cutting steels--Part 3: Case-hardening steels
Standard ISO 683-3-2019 Heat-treatable steels,alloy steels and free-cutting steels--Part 3: Case-hardening steels
Standard DIN EN 10084-2008 Case hardening steels – Technical delivery conditions
Standard ISO 683-11-2012 Case-hardening steels
Standard NF EN 10084-2008 Surface hardened structural steel


Chemical Composition(%)


Standard Material Designation Chemical Composition (%)
EN 10084-1998
Case hardening steels. Technical delivery conditions
1.6566
(17NiCrMo6-4)
 
Min
Max
DIN EN ISO 683-3-2019
Heat-treatable steels,alloy steels and free-cutting steels--Part 3: Case-hardening steels
17NiCrMo6-4
 
Min
Max
DIN EN 10084-2008
Case hardening steels – Technical delivery conditions
17NiCrMo6-4
(1.6566)
 
Min
Max
ISO 683-3-2019
Heat-treatable steels,alloy steels and free-cutting steels--Part 3: Case-hardening steels
17NiCrMo6-4
 
Min
Max
ISO 683-11-2012
Case-hardening steels
17NiCrMo6-4
 
Min
Max
NF EN 10084-2008
Surface hardened structural steel
17NiCrMo6-4
(1.6566)
 
Min
Max
For Reference Only